UHP 700mm Graphite Electrode
700mm UHP graphite electrode an yi shi da babban coke mai allura mai inganci, wanda aka kafa, gasasshe, mai ciki, graphitized da injin sarrafa kayan masarufi a matsayin babban kayan sarrafawa don tanderun wutar lantarki. UHP 700mm graphite electrode, The allowable halin yanzu iya aiki ne 73000 ~ 96000A, da yarda halin yanzu yawa ne 18-24A/㎡ . An ƙera shi don ƙera ƙarfe mai ƙarfi na baka ta wutar lantarki.
Lura: Ana ba da shawarar cewa ƙarfin halin yanzu ya kasance -10% don wutar lantarki da + 10% don tanderun ladle.
Kwatanta Bayanin Fasaha don UHP Graphite Electrode 28" | ||
Electrode | ||
Abu | Naúrar | Specific mai bayarwa |
Halayen Halayen Sanda | ||
Diamita na Ƙa'ida | mm | 700 |
Max Diamita | mm | 714 |
Min Diamita | mm | 710 |
Tsawon Suna | mm | 2200-2700 |
Matsakaicin Tsayin | mm | 2300-2800 |
Min Tsawon | mm | 2100-2600 |
Yawan yawa | g/cm3 | 1.68-1.72 |
Ƙarfin mai juzu'i | MPa | ≥ 10.0 |
Young' Modul | GPA | ≤13.0 |
Takamaiman Juriya | µΩm | 4.5-5.4 |
Matsakaicin yawa na yanzu | KA/cm2 | 18-24 |
Ƙarfin ɗauka na Yanzu | A | 73000-96000 |
(CTE) | 10-6 ℃ | ≤1.2 |
abun cikin toka | % | ≤0.2 |
Halayen Halayen Nono (4TPI) | ||
Yawan yawa | g/cm3 | 1.80-1.86 |
Ƙarfin mai juzu'i | MPa | ≥24.0 |
Young' Modul | GPA | ≤20.0 |
Takamaiman Juriya | µΩm | 3.0 zuwa 3.6 |
(CTE) | 10-6 ℃ | ≤1.0 |
abun cikin toka | % | ≤0.2 |
Ƙaunar halin yanzu da ake ba da izini don na'urorin lantarki na graphite masu ƙarfi | |||||
mara iyaka diamita | halattaccen halin yanzu | mara iyaka diamita | halattaccen halin yanzu | ||
mm | A | A/㎡ | mm | A | A/㎡ |
250 | 9000 ~ 14000 | 18 zuwa 25 | 500 | 38000 ~ 55000 | 18 zuwa 27 |
300 | 15000-22000 | 20 zuwa 30 | 550 | 45000 ~ 65000 | 18 zuwa 27 |
350 | 20000-30000 | 20 zuwa 30 | 600 | 52000 ~ 78000 | 18 zuwa 27 |
400 | 25000-40000 | 16 zuwa 24 | 650 | 70000 ~ 86000 | 21 zuwa 25 |
450 | 32000 ~ 45000 | 19 zuwa 27 | 700 | 73000 ~ 96000 | 18 zuwa 24 |
Ultra high power graphite electrode da haɗin gwiwa misali | |||||
abubuwa | naúrar | diamita mara kyau (mm) | |||
250 ~ 400 | 450 ~ 550 | 600 ~ 700 | |||
takamaiman juriya | electrode nono | μ Ω•m | 4.8-5.8 3.4-4.0 | 4.5-5.6 3.4-3.8 | 4.5 ~ 5.4 3.0 ~ 3.6 |
Ƙarfin mai juzu'i | electrode nono | MPa | ≥12.0 ≥22.0 | ≥12.0 ≥22.0 | ≥10.0 ≥24.0 |
na roba modules | electrode nono | GPA | ≤13.0 ≤18.0 | ≤13.0 ≤18.0 | ≤13.0 ≤20.0 |
abun cikin toka | electrode nono | % | ≤0.2 | ≤0.2 | ≤0.2 |
yawa yawa | electrode nono | g/m³ | 1.68 zuwa 1.73 1.78 zuwa 1.84 | 1.68 zuwa 1.72 1.78 zuwa 1.84 | 1.68 ~ 1.72 1.80 ~ 1.86 |
(CTE) | electrode nono | 10 ℃ | ≤1.2 ≤1.0 | ≤1.2 ≤1.0 | ≤1.2 ≤1.0 |